Cold Soldering, Over-Soldering, and Grid Breakage in Solar Modules

Release time:2025-12-06

Release time:2021-09-15

Author:

Author:


In the production of solar modules, string welding is one of the most critical steps. The current mainstream welding method uses infrared heating lamps to heat the soldering strips, while a pressure fixture applies force to ensure the solder strip is welded onto the cell's busbars. The heat melts the tin–lead alloy on the solder strip, which then combines with the silver paste on the cell's busbars and pad points, forming a metallic alloy bond. The quality of the weld directly affects the module's performance and efficiency. However, during production, several defects may occur, such as cold soldering, over-soldering, and grid breakage.

 

Cold Soldering: Inadequate Fusion of Solder and Silver Paste

Cold soldering occurs when the tin–lead solder and silver paste do not fully melt or fuse together, resulting in a weak and unreliable weld.

 

EL testing machine

 

Causes: Insufficient welding temperature, short welding time, inadequate welding pressure, or issues with flux such as oxidation.

Impacts: Cold soldering increases resistance at the weld point, causing localized heating and reducing the module’s power output. In severe cases, it can burn the solar cell, damage the EVA film, and even lead to fire hazards.

 

Over-Soldering: Excessive Heat and Time Leading to Damage

Over-soldering occurs when the welding temperature is too high or the welding duration is too long, causing the silver electrode paste on the cell to separate from the silicon substrate, increasing electrical resistance.

Causes: Excessively high welding temperatures, prolonged welding times, excessive equipment pressure, or improper equipment calibration.

Impacts: Over-soldering can cause mechanical damage to the cell, such as fractures or microcracks. Excessive heat may burn the silver paste grid, resulting in electrical short circuits and reducing the overall lifespan of the solar module.

 

Grid Breakage: Disruption of Current Flow Due to Broken Grid Lines

Grid breakage, also known as “busbar breakage”, refers to fractures or missing sections of the metal grid lines—typically made of silver paste—on the front or back of the solar cell. This disrupts or blocks current transmission.

 

Types of Grid Breakage

  • Visible Grid Breakage:

Occurs when the grid lines are not fully printed due to issues during the screen-printing process, such as mesh blockages, uneven squeegee pressure, or improper printing parameters.

 

  • EL Grid Breakage:

Occurs when the grid lines fail to form a proper silver–silicon alloy during sintering, leading to increased resistance and reduced current-collection capability. This defect is detectable through electroluminescence (EL) testing.

 

                

Causes: Printing blockages, uneven squeegee pressure, improper sintering temperature profiles, contamination on the silicon surface, or existing defects such as microcracks that expand during processing. Improper handling during later steps—such as welding, lamination, or transportation—can also cause grid breakage.

Impacts: Grid breakage reduces the effective power-generating area of the solar cell, and the current generated near the damaged region cannot be efficiently collected. This increases transmission losses. Severe grid breakage may cause local cell failure and create hot spots.

 

New Choice

Chintiyan has been deeply engaged in the photovoltaic industry for many years, focusing on continuous technological innovation and R&D of PV manufacturing equipment. Leveraging strong development capabilities and advanced production systems, the company has introduced a new generation of high-precision string welding machines—such as the High-Speed BC Stringer Machine CTM-60BC, the Low-Speed BC Stringer Machine CTM-15BC, and many other models. These machines are designed to effectively address key welding defects commonly found in module production, including cold soldering, over-soldering, and grid breakage.

The equipment features high-accuracy thermal control, intelligent pressure management, and programmable process parameters to ensure stable and reliable alloy bonding between solder ribbons and solar cells. This minimizes defect occurrence at the source while improving welding consistency and electrical performance.

In addition, Chintiyan's string welding systems can be fully customized based on different cell technologies, process routes, and production line speeds, enabling module manufacturers to achieve higher product quality, improved yield rates, and greater production efficiency. With continuous technological advancement and extensive industry experience, Chintiyan is committed to delivering more reliable and efficient equipment solutions to the global PV industry—driving the sector toward higher quality and higher performance.

 

Conclusion

The quality of string welding plays a critical role in the overall performance of solar modules. Cold soldering, over-soldering, and grid breakage can significantly impact both electrical performance and long-term reliability. Addressing welding defects is not only about improving production quality—it is essential for ensuring system durability and building trust in solar technology. With continuous innovation and stricter quality standards, the industry can move toward a more efficient and sustainable energy future.