Effective Solution for Bubbles in PV Modules After Lamination
Release time:2025-11-12
Release time:2021-09-15
Author:
Author:
Bubbles appearing in PV modules after lamination can be caused by various factors, including raw materials, equipment, environment, and human operation. Below is a detailed analysis of the causes and corresponding solutions.
Ⅰ. Material Abnormalities
1.Positioning Tape Bubbles: Bubbles related to positioning tape are generally caused by a mismatch between the lamination parameters (primarily temperature and pressure) and the tape characteristics. This can be resolved by adjusting the lamination parameters or replacing the positioning tape.
2.Encapsulant Film Abnormalities: Bubbles due to encapsulant film abnormalities are usually caused by the presence of "dead material" (e.g., partially cured or degraded resin) within the film, or issues like local lack of adhesive or low grammage (weight per unit area).
•Material-related issues can typically be solved by replacing the problematic material. If it's uncertain whether the material is the cause, cross-verification by replacing materials can help identify the specific abnormal material.
Ⅱ. Equipment Abnormalities
1.Air Leakage: If the laminator leaks after the lid is closed, it can cause bubbles. The cause is that during vacuum pumping, air enters the chamber from the leak point, leading to insufficient vacuum levels in that area and preventing bubbles from being evacuated from the module.
•For air leaks, it is necessary to inspect the laminator's sealing rings, vacuum pump, vacuum pipes, and other components. Also, check if the lid is properly closed and if any foreign objects are obstructing the sealing ring or the upper chamber flange.
2.Temperature: If the lamination process parameters are correct, but bubbles (not snow pattern bubbles) appear consistently on the front side of the module (the side facing the hot plate during lamination) at a fixed machine location.
•Check if localized overheating on the laminator's heating plate is causing premature cross-linking of the encapsulant in that specific area, leading to bubbles.
Ⅲ. Human Operation
Improper Film Placement: During film laying, incorrect parameter settings by operators can lead to the encapsulant film being cut too short, misaligned, or missing border strips. This can cause a lack of adhesive at the module edges, resulting in bubbles after lamination.
•Check the EL image to determine if the issue is related to improper film placement.
Ⅳ. Environmental Issues
1.High Encapsulant Moisture Content: If the encapsulant film is stored in a high-humidity environment for an extended period, it can absorb moisture. This leads to small bubbles after lamination, typically scattered without a fixed pattern or location.
2.Foreign Object Bubbles: Bubbles caused by foreign objects like insects indicate that the workshop environment does not meet standards. Solutions include enforcing strict door closure protocols for personnel entering/exiting the workshop and implementing pest control measures.
Previous Page