How to Solve Weak Welding Issues in PV String Welding Machines?

Release time:2025-06-11

Release time:2021-09-15

Author:

Author:


Weak welding (cold solder joints) is one of the most common quality challenges in photovoltaic (PV) module manufacturing. If not addressed promptly, it can lead to power loss, reliability risks, and reduced module lifespan. This article outlines practical identification methods, root causes, and effective solutions to help manufacturers improve string welding quality and production stability.

 

1. Weak Welding (Cold Solder)

(1) Visual Inspection

Observe the cell string at an angle of approximately 30°. Uneven solder joints, dull surfaces, or incomplete wetting often indicate weak welding.

(2) Electroluminescence (EL) Detection

By capturing and stitching EL images, weak welding points can be identified. Symmetrical dark areas along the main grid lines are a typical sign of insufficient solder bonding.

 

2. Root Causes and Targeted Solutions

(1) Temperature-Related Issues

Cause: Welding temperature too low or heating time insufficient.

Solution: Increase infrared lamp power and extend welding time for affected zones.

(2) Flux-Related Problems

Causes & Solutions:

Low flux concentration → Increase drying temperature

Sponge degradation → Replace sponge regularly

Flux drying out → Inspect and stabilize the flux replenishment system

(3) Pressure Pin Abnormalities

Cause: Loose, stuck, or misaligned pressure pins.

Solution: Inspect pressure pins and adjust pin position and ensure stable contact pressure.

(4) Ribbon & Silver Paste Issues

Insufficient tin coating → Reduce ribbon stretch ratio and inspect scraping channels

Incompatible silver paste → Replace affected cells to avoid recurring defects

 

3. Equipment Operation Abnormalities

(1) Conveyor Belt Misalignment

Belt deviates inward → Rotate the outer screw clockwise

Belt deviates outward → Rotate the inner screw clockwise

Adjust gradually until the belt runs straight.

(2) Rotary Table Air Hose Tangling

Run the machine until B/C rotary table hoses are fully untangled.

(3) Insufficient Air Pressure

Inspect the air compressor, pneumatic circuits, and pressure regulator for stability.

 

4. Ribbon & Material-Related Issues

(1) Twisted or Exposed Ribbon (White Spots)

Stop the machine immediately

Inspect the buffer device and straighten the ribbon

(2) Excessive Solder on Ribbon

Reduce preheating plate temperature by 5–10°C

Adjust pressure pin force accordingly

(3) Ribbon Exposure Control

Clean ribbon clamps 1–2 times per hour

Adjust pressure pin height and ribbon guide slots precisely

 

5. Other Common Welding Faults

(1) Uneven Cell Spacing

Check air valve pressure

Clean the welding table

Remove residual flux

(2) Misaligned Ribbon Starting Point

Optimize welding power and time

Adjust baffle position if necessary

(3) Ribbon Bowing

Clean the Z-punching mold and rear pressure claws

Fine-tune the Z-punching position knob

(4) Front Ribbon Protrusions

Remove solder residue from pressure pins

Re-adjust pin pressure to ensure uniform bonding

 

6. Conclusion

Stable welding quality in PV string welding machines depends on precise temperature control, reliable pressure systems, proper material matching, and regular equipment maintenance. By systematically identifying weak welding symptoms and applying targeted corrective actions, manufacturers can significantly improve module reliability, yield, and long-term performance.